Nanhaiya vaega sikuli paelo ua atiaʻe mo faʻatasi faʻataʻamilomilo extruders masaga, maua modular fetuutuunai ma faigofie tausiga. Fa'atūina i le 2014, fa'atasia e Nanhaiya fa'atekonolosi fa'ato'aga a Europa e tu'uina atu ai vaifofo pa'u sikulima umi ma lelei mo le fa'afefiloi ma le gaosiga o masterbatch.

O le vaega sikulima pa'u faiga e mafai ai elemene aoga eseese-e pei o le felauai, fefiloi, ma lomi vaega-ina ia saoloto tuufaatasia e tusa ai ma manaoga faagasologa. O vaega taʻitasi e faia i le uamea faʻafefete faʻafefete, e tuʻuina atu ai le maʻaʻa mataʻina, malosi maualuga, ma le ofuina o le teteʻe. O le mamanu faʻapitoa e mafai ai ona sui vave o vaega ua masaesae, faʻaitiitia taimi faʻaletonu ma faʻaitiitia tau o le tausiga. O paʻu faʻapitoa a Nanhaiya e fetaui ma faʻailoga faavaomalo e pei o Coperion ma JSW.

Fua Fa'atatau

Mea

38CrMoAlA,SKD61

Maaa Togafitiga vevela

HB260-320

Maaa ole Nitriding

HV950-1000

Nitriding loloto

0.50-0.70mm

Nitriding Brittleness

≤vasega 1

Talatala

Ra0.4

Fa'asa'o o le Siu

0.015mm

Maaa ole Fa'apalapala Chrome

HV≥950HV

Chrome Mafiafia

0.05-0.10mm

Maaa Bimetal

HRC60-65

Bimetal loloto

2.0-3.0mm

Faiga Fa'atauga ma Fa'aoga

Nanhaiya vaega sikuli paelo maua fetuutuunai, tumau, ma le faatinoga maualuga. O le mamanu fa'avasegaina e mafai ai e tagata fa'aoga ona fetu'una'i le fa'atulagaina o sikulima e tusa ai ma fa'asologa o meafaitino po'o le fa'agaioiina o le fa'amoemoega, fa'ataunu'uina le fa'apipi'iina lelei, fa'afefiloi, ma le fa'asalalauina. E faʻaaogaina lautele i palasitika inisinia, faʻapipiʻi faʻatumu, masterbatch, ma faʻapipiʻi faʻaopoopo.

Segment Screw Barrel Segment Screw Barrel Segment Screw Barrel Segment Screw Barrel Segment Screw BarrelSegment Screw Barrel

Fa'amatalaga o gaosiga

O vaega ta'itasi o Nanhaiya pa'u sikulima o lo'o fa'agaioia e le CNC ma fa'amama le vevela vevela. E mafai ona sui ta'ito'atasi laina i totonu, fa'aleleia atili le tau. Alloy coatings o lo'o fa'aogaina i luga o vaega maualuluga e fa'alautele ai le ola tautua. Nanhaiya segmented system e tuʻuina atu le faʻaogaina mautu, tausiga faigofie, ma le faʻatuatuaina umi, fesoasoani i tagata faʻatau e faʻaauau pea le gaosiga o le extrusion maualuga.

Segment Screw BarrelSegment Screw BarrelSegment Screw BarrelSegment Screw BarrelSegment Screw BarrelSegment Screw Barrel
Auina atu Su'esu'ega
Fa'amatalaga Fa'afeso'ota'i
Fa'afeiloa'i i la matou upega tafa'ilagi! Mo fa'amatalaga e uiga ia matou oloa po'o le lisi o tau, fa'amolemole tu'u lau imeli ia i matou ma o le a matou feso'ota'i i totonu ole 24 itula.
X
Matou te fa'aogaina kuki e ofo atu ai ia te oe se su'esu'ega sili atu, au'ili'ili fefa'ataua'iga i luga ole laiga ma fa'avasega mea e aofia ai. I le fa'aogaina o lenei 'upega tafa'ilagi, e te ioe i le matou fa'aogaina o kuki. Faiga Fa'alilolilo
TeenaTalia